Factory-direct manufacturer · 16 patents · Free samples & full English TDS

info@fotomaterial.com +86 133 8220 9786

FOTO New Material
FT-GFMK-401 Mg-K Granular Refining Flux (Na-Free, F-Free)
  • Eco / low smoke
  • Fluoride-free
  • Sodium-free

FT-GFMK-401 Former code: GFMK101 Granular Refining Fluxes

FT-GFMK-401 Mg-K Granular Refining Flux (Na-Free, F-Free)

Our flagship remelt granular flux: sodium-free and fluoride-free, melts below 500°C, removes Na ≥ 85%, Ca ≥ 75%, Li ≥ 50% with a dry, loose dross.

Form
Granular
Dosage
1.0–1.5 kg/t-Al
Temperature
710–780°C
Packaging
Woven bags or cartons with PE liner, 20 kg or 25 kg per bag

Alloys: 1xxx Pure Al3xxx Al-Mn6xxx Al-Mg-Si8xxx Al-Li/Other

  • Free sample for trials
  • English TDS & SDS
  • Factory-direct export

Product overview

FT-GFMK-401 is a sodium-free, fluoride-free remelt granular refining flux that eliminates sodium embrittlement and fluoride corrosion while staying smoke-free. With a melting point below 500°C it melts instantly when injected and reacts fully.

It removes alkali metals with high efficiency — Na ≥ 85%, Ca ≥ 75%, Li ≥ 50%. After refining the dross is loose and dry, giving clean metal/dross separation and low aluminium loss.

Technical data

Product codeFT-GFMK-401
AppearanceWhite or light-grey granules
Particle size0.8–3.35 mm
Melting point≤ 500°C
Moisture≤ 0.5%
Na removal≥ 85%
Ca removal≥ 75%
Li removal≥ 50%
Recommended dosage1.0–1.5 kg/t-Al
Working temperature710–780°C

Values are typical. Optimum dosage depends on melt cleanliness, scrap ratio and quality targets — confirm by sampling. Custom particle sizes and packaging available.

Applications

  • 1xxx pure aluminium
  • 3xxx Al-Mn alloys
  • 6xxx Al-Mg-Si alloys
  • 8xxx Al-Li alloys
  • High-end alloys with strict Na and F limits

How to use

  1. Injection (recommended): with dry N₂ or Ar inject the granules deep into the melt, lance tip at 2/3 melt depth, moving horizontally without touching the walls.
  2. Rotary degasser: add slowly into the stable vortex.
  3. Refining time 8–20 min.
  4. Stand 15–20 min, then skim the surface dross.

Packaging, storage & safety

Packaging
Woven bags or cartons with PE liner, 20 kg or 25 kg per bag
Shelf life & storage
12 months unopened. Store indoors in a ventilated, dry place away from fire and acids. If damp, dry at 150°C and pass a 5-mesh sieve before use.
Notes & safety
  • Wear dust mask, goggles and heat-resistant gloves. Beware of metal splash and keep the shop ventilated.

Request a quote, TDS or free sample for FT-GFMK-401

We use your details only to answer this enquiry. No spam, no sharing.

Need a flux recommendation for your alloy?

Our metallurgists reply within one working day — with the right product, TDS and a free sample.