Factory-direct manufacturer · 16 patents · Free samples & full English TDS

info@fotomaterial.com +86 133 8220 9786

FOTO New Material
FT-GFNM-501 Potassium-Free Granular Refining Flux for 6xxx
  • Fluoride-free
  • Potassium-free

FT-GFNM-501 Former code: GFNM201 Granular Refining Fluxes

FT-GFNM-501 Potassium-Free Granular Refining Flux for 6xxx

Economical NaCl-MgCl₂ granular flux, potassium-free and fluoride-free — protects the surface finish of 6063 and other 6xxx alloys.

Form
Granular
Dosage
0.8–1.2 kg/t-Al
Temperature
720–760°C
Packaging
Woven bags or cartons with PE liner, 20 kg or 25 kg per bag

Alloys: 6xxx Al-Mg-Si

  • Free sample for trials
  • English TDS & SDS
  • Factory-direct export

Product overview

FT-GFNM-501 is potassium-free, avoiding any potential effect of potassium on the surface treatment of 6xxx alloys such as 6063. The sodium chloride – magnesium chloride system delivers good degassing and drossing at an economical cost.

Three-in-one function, smoke-free, fluoride-free and hexachloroethane-free.

Technical data

Product codeFT-GFNM-501
AppearanceWhite granules
Particle size0.8–3.35 mm
Melting point≤ 500°C
Recommended dosage0.8–1.2 kg/t-Al
Working temperature720–760°C

Values are typical. Optimum dosage depends on melt cleanliness, scrap ratio and quality targets — confirm by sampling. Custom particle sizes and packaging available.

Applications

  • 6xxx alloys: 6061, 6063, 6005
  • Other potassium-sensitive low-Mg alloys

How to use

  1. Inject deep into the melt.
  2. Stand 15 min and skim.

Packaging, storage & safety

Packaging
Woven bags or cartons with PE liner, 20 kg or 25 kg per bag
Shelf life & storage
12 months unopened. Store indoors in a ventilated, dry place away from fire and acids. If damp, dry at 150°C and pass a 5-mesh sieve before use.
Notes & safety
  • Contains sodium — never use for 5xxx or 7xxx high-Mg alloys.
  • Wear dust mask, goggles and heat-resistant gloves. Beware of metal splash and keep the shop ventilated.

Request a quote, TDS or free sample for FT-GFNM-501

We use your details only to answer this enquiry. No spam, no sharing.

Need a flux recommendation for your alloy?

Our metallurgists reply within one working day — with the right product, TDS and a free sample.